人工晶体学报 ›› 2010, Vol. 39 ›› Issue (2): 350-354.
陈江恩;刘保亭;孙杰;郭延岭;马蕾;娄建忠;彭英才
CHEN Jiang-en;LIU Bao-ting;SUN Jie;GUO Yan-ling;MA Lei;LOU Jian-zhong;PENG Ying-cai
摘要: 采用磁控溅射法和脉冲激光沉积法,在SrTiO3(001)衬底上制备了La0.5Sr0.5CoO3(70 nm)/Pb(Zr0.4Ti0.6)O3(70 nm)/La0.5Sr0.5CoO3(70 nm) (LSCO/PZT/LSCO)铁电电容器异质结.X射线衍射结果表明:LSCO和PZT薄膜均为外延结构.在5 V的外加电压下, LSCO/PZT/LSCO电容器具有较低的矫顽电压(0.49 V),较高的剩余极化强度(41.7 μC/cm2 )和较低的漏电流密度(1.97×10-5 A/cm2),LSCO/PZT/LSCO电容器的最大介电常数为1073.漏电流的分析表明:当外加电压小于0.6 V时,电容器满足欧姆导电机制;当外加电压大于0.6 V时,符合空间电荷限制电流(SCLC)导电机制.
中图分类号: