纳米级SnO2或Yb2O3对熔融石英陶瓷析晶性能的影响

谷莹蕾1,2, 李勇1, 卜景龙2, 马超3, 王志发2   

  1. 1.华北理工大学轻工学院,唐山 064000;
    2.华北理工大学材料科学与工程学院,河北省无机非金属材料重点实验室,唐山 063210;
    3.唐山时创高温材料股份有限公司,唐山 064000
  • 收稿日期:2021-02-19 出版日期:2021-05-15 发布日期:2021-06-15
  • 作者简介:谷莹蕾(1986—),女,河北省人,讲师。E-mail:490557762@qq.com
  • 基金资助:
    国家自然科学基金(51072046)

Effect of Nano-SnO2 or Nano-Yb2O3 on Crystallization Property of Fused Quartz Ceramics

GU Yinglei1, 2, LI Yong1, BU Jinglong2, MA Chao3, WANG Zhifa2   

  1. 1. Qinggong College, North China University of Science and Technology, Tangshan 064000, China;
    2. Hebei Provincial Key Laboratory of Inorganic Nonmetallic Materials, College of Materials Science and Engineering, North China University of Science and Technology, Tangshan 063210, China;
    3. Tangshan Strong Refractories Co., Ltd., Tangshan 064000, China
  • Received:2021-02-19 Online:2021-05-15 Published:2021-06-15

摘要: 通过XRD分析和热膨胀率实验,从析晶角度探讨了添加纳米级SnO2或Yb2O3对熔融石英陶瓷析晶性能的影响。结果表明:熔融石英陶瓷高温析晶的主要晶化产物为方石英,方石英析出量随烧结温度的提高而逐渐增多;纳米级SnO2或Yb2O3的引入可通过抑制熔融石英中方石英的析出,有效地降低熔融石英材料在升温过程中的热膨胀率,并且随着烧结温度升高需要不断调整添加剂用量,纳米级SnO2和Yb2O3的最佳用量(质量分数)分别为1%和2%。

关键词: 熔融石英陶瓷, 析晶, 纳米级SnO2, 纳米级Yb2O3, 热膨胀率

Abstract: Effects of nano-SnO2 or nano-Yb2O3 on crystallization property of fused quartz ceramics were studied by XRD and measurement of thermal expansion rate from the perspective of crystallization. The results indicate that cristobalite as the main crystal phase would crystallized in the fused quartz glass at high temperature, and the amount of cristobalite increases with increasing of sintering temperature; the addition of nano-SnO2 or nano-Yb2O3 effectively decreases the expansion ratio of the fused quartz ceramic materials during temperature elevating process by inhibiting crystallization of cristobalite, and with increase of sintering temperature, the dosage of additive necessary to keep the fused quartz ceramic materials with a low expansion ratio was adjusted, the optimum dosage (mass fraction) of nano-SnO2 or nano-Yb2O3 as crystallization inhibitors is 1% and 2%, respectively.

Key words: fused quartz ceramics, crystallization, nano-SnO2, nano-Yb2O3, thermal expansion